Material Specifications
TEST TYPE | EPDM | SILICONE |
---|---|---|
Advance Ozone Resistance
(Test at 500 pphm) |
||
70 hours | 70 hours | |
High Temperature | ||
Intermittent: | 275+ °F | 500+ °F |
Continuous: | 212+ °F | 437+ °F |
Low Temperature |
|
|
Resistance Tested to: | 65- °F | 100- °F |
Tensile Strength: | 1,450 psi | 700 psi |