Material Specifications
TEST TYPE | EPDM | SILICONE |
---|---|---|
Advance Ozone Resistance
Test at 500 pphm |
70 hours | 70 hours |
High Temperature | ||
Intermittent: | 275+ degrees F | 500+ degrees F |
Continuous: | 212+ degrees F | 437+ degrees F |
Low Temperature |
|
|
Resistance Tested to: | 65- degrees F | 100- degrees F |
Tensile Strength: | 1,450 psi | 700 psi |